BRENT ANFINSON on thu 13 feb 97

I discovered a while ago that I can repair cracks in bisque with a
combination of powdered bisque and a bit of glaze mixed to a thick
paste.I smear it over the crack, then when it's dry I sand it down. Then
depending on if its glaze or underglaze I fire it accordingly.I've
really had a very good success rate with this.It just depends on how
much work I've put into a piece already if I choose to use this
technique. Good luck M.