please would a techno-artist-potter-craftsperson please do an analysis with
your computer and a glaze program and tell me, based on todays materials,
and a computer---does this formula still stand up.

I have used it for 33 years as my base glaze, have altered it, stretched it,
fudged it, and love it.

just for fun and interest.. Mel Jacobson

Rhodes 32 cone 10 butter matt

Feldspar 48.9
China Clay 25.1
Dolomite 22.4
Whiting 3.5

you may e-mail me any results... thanks

Ron Roy on sat 30 mar 96

>----------------------------Original message----------------------------
>please would a techno-artist-potter-craftsperson please do an analysis with
>your computer and a glaze program and tell me, based on todays materials,
>and a computer---does this formula still stand up.
>
>I have used it for 33 years as my base glaze, have altered it, stretched it,
>fudged it, and love it.
>
>just for fun and interest.. Mel Jacobson
>
>Rhodes 32 cone 10 butter matt
>
>Feldspar 48.9
>China Clay 25.1
>Dolomite 22.4
>Whiting 3.5
>
>you may e-mail me any results... thanks

Hey Mel,

Need to know what feldspar and what kaolin
and better include which dolomite and whiting.