Emily Henderson on thu 5 jun 97
Much thanks to Ron Roy and Dave Hewitt and Karl Platt who responded to my
questions about expansion and my forays into the low expansion glaze world.
Right now I'm just starting to make the greenware for my next kiln load so I
won't be able to test at ^8 again for a while. But I've really got some
good ideas to try. AND Ron? Tacoma or Lynnfield? Please Glazes...please,
CHEAP. I know you're worth a fortune but unless I get some good stuff comin
out at ^8 or the weather clears for a pitfire, I ain't gonna eat other than
at my "day-job" Emily in Astoria where the sun is peeking just before
setting but isn't really ready to make a commitment yet.
| |
|