> I don't have much experience but maybe this can help. The saw dust
should not burn out for 9 hrs. Maybe it ther wasn't enough? Also was it
literally dust? Maybe the pieces weren't big enough so they burn out too
fast. There shouldn't be a great big flame but make sure it is still lit
after a few minutes.
>
| |
|