Hi,

Why don't you make your own and add stains? Rose Red is a bright red stain
from US Pigment and pansy is a deep purple from Mason. John Kenney has a
good slip recipe that I've used to make underglazes. It's in his book named
I think the Complete Book of Pottery. Anyway, the Potter's Shop carries this
book.

Linda
Ithaca, NY

PS, using this slip and any other than I make, I can glaze right over the
piece without firing first. I have not been able to do this with the