I coated fiber lining our castable door in the soda kiln using
ITC (INternational Tech. Ceramics). It works great. Fiber is unscathed.
It is sold thru Axners or directly from ITC in Pontevedra Fla.
They will also have a booth at NCECA. Great stuff! and very helpful
people.