Lisa on fri 4 oct 96
Anyone know a source for Ferro Frit 3185? I have tried ART, Axner,
Kickwheel, Minnesota Clay Co., Highwater, and Amaco with no luck.
Lisa in Greensboro, where there is some sort of weird yellow orb lighting
up the world.
Karen Gringhuis on fri 4 oct 96
Try Standard Cer. Supply in Pittsburg or Laguna in Los Angeles(?) - both
have been quite knowledgeable for me. Or Call Tom Turnbull at Midsouth
Cer. Supply (?) in Memphis - he could probably order if he doesn't have.
He's a good guy.
Shelley S. on sat 5 oct 96
Lisa,
Frit 3185 is in the Sheffield Clay Catalog. Their number is 413-229-7700.
The catalog I have is a few years old, but maybe they still have it.
Shelley
----------
From: Lisa[SMTP:lpskeen@nr.infi.net]
Sent: Friday, October 04, 1996 7:07 AM
To: Multiple recipients of list CLAYART
Subject: Source for frit 3185
----------------------------Original message----------------------------
Anyone know a source for Ferro Frit 3185? I have tried ART, Axner,
Kickwheel, Minnesota Clay Co., Highwater, and Amaco with no luck.
Lisa in Greensboro, where there is some sort of weird yellow orb lighting
up the world.
Erich on sun 6 oct 96
Shelley S. wrote:
>
> ----------------------------Original message----------------------------
> Lisa,
>
> Frit 3185 is in the Sheffield Clay Catalog. Their number is 413-229-7700.
> The catalog I have is a few years old, but maybe they still have it.
>
> Shelley
>
> ----------
> From: Lisa[SMTP:lpskeen@nr.infi.net]
> Sent: Friday, October 04, 1996 7:07 AM
> To: Multiple recipients of list CLAYART
> Subject: Source for frit 3185
>
> ----------------------------Original message----------------------------
> Anyone know a source for Ferro Frit 3185? I have tried ART, Axner,
> Kickwheel, Minnesota Clay Co., Highwater, and Amaco with no luck.
>
> Lisa in Greensboro, where there is some sort of weird yellow orb lighting
> up the world.
Hi Lisa ,
I just got a fax from Laguna Clay in L.A. and Ferro Frit 3185 is the first frit
on the list.
3185, Mol. Wt. 807.2, Na2O 1000, B2O3 4.43, SiO 7.27 , Temp.F. 1350
Call Laguna Clay 1.800.452.4862
Erich Broennimann
Ocean View, HI
808.939.7281
| |
|