EDWIN GOULD on mon 13 jan 97
I looking for a published design of a simple, inexpensive hood and
exhaust blower for spraying glaze on my ceramic pieces. Any tips out
there? Size and make of a good blower/exhaust fan? Thanks
edgould@erols.com
Kirk Morrison on wed 15 jan 97
On 13 Jan 97 at 19:29, EDWIN GOULD wrote:
> ----------------------------Original message----------------------------
> I looking for a published design of a simple, inexpensive hood and
> exhaust blower for spraying glaze on my ceramic pieces. Any tips out
> there? Size and make of a good blower/exhaust fan? Thanks
> edgould@erols.com
>
>
I took an old oven hood and made one with a couple of muffin fan motors
from a surplus electronics store a few years back worked great on my
spray booth. I added sides from the materials from a old dryer. Cost
$12 I could have used plywood but I got the dryer for free.
Kirk
| |
|