NELS LINDE/KAREN FREDRICKSON on thu 12 jun 97
------------------
----------------------------Original message----------------------------
.. Frequently I get small specks which fire black.
............................... Does anyone have any suggestions on how I =
can
rectify this
problem?
Thanks in advance.
Grace
I spray underglazes a lot and if I get black spots it is usually some dried
black in your airbrush. It happens with other colors as well. It just =
doesn't
show up easily. Try soaking it overnight and a thorough cleaning.
Good luck=21
Nels Linde
hawkdanc=40spacestar.net
| |
|