Tony Hansen on tue 6 aug 96

>Ron Pothier: I am looking for a substitute for the frit 3841 which I am told
>is discontinued.

Here's what I have on frit 3481:

FRIT 3481 - MEDIUM LEAD HIGH LIME GLAZE FRIT

CaO....... 9.90% [ 0.52]
K2O....... 1.19% [ 0.04]
Na2O...... 3.09% [ 0.15]
PbO....... 22.77% [ 0.30]
B2O3...... 6.20% 0.26
Al2O3..... 7.00% 0.20
SiO2...... 49.86% 2.43

Cone Range: 06-02
Suitable for chrome tin pink and maroon colors.
Sub: O.Hommel 403
Made from flint, borax, calcium, clay and lead.

--