search  current discussion  categories  events - adjudicating 

subject: re: jiffy mixers & the competition

updated fri 24 oct 97

 

Joseph Herbert on fri 3 oct 97

Coriene Null indicated that toilet brushes were somehow wasteful of glaze.
this may be true if you have one and use it for several glazes - washing in
between. If you buy ONE FOR EACH glaze bucket, this is not true. For $1.00
each, it's a pretty good deal. the plungers get limber and useless after
some time in the glaze and can't get even part of a cake of glaze off the
bottom of the trash can.

Buy lots of brushes and just leave then in there. Cheapest and best way to
do it.

Joe