From my RISD undergrad days....

Boubaric Tesha (still don't understand this name) Cone 9-10 R and Salt


Kona F-4 spar 21.0
Whiting 16.0
Ball Clay 26.0
Flint 26.0
Red Iron Oxide 12.0

Good Luck