Ron Roy on mon 20 jan 97

And yet another addition to my post on durability testing. Tom Buck kindly
reminded me that I should have added - Your vinegar is usually a 5%
solution of acetic acid - the consentration should be right on the bottle -
my white and cider are both 5%

Ron Roy