Russel Fouts on fri 6 dec 96
Janet,
>> I also saw the note in CM about using just vinegar instead of doing
slipping and scoring. I had a piece where a joint had separated
during unskilled drying so I figured I'd try out the vinegar thing.
I took powdered clay body and mixed in a little vinegar <<
I join all my handbuilt pieces this way and never score the clay, I just use
vinegar and my clay body, Peggy Heer adds Karo syrup (? something sweet anyway)
to the vingar and clay and calls it spooze.
Works great, smells like pickles.
Russel (Panic level: Code Red. Open Studio TOMORROW!!!)
=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=
* Russel Fouts, CI$: 100021,23,
Bruxelles, Belgium
Internet: 100021.23@CompuServe.Com
"It took more then one man to change my name to Shanghai Lil."
MD
-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-
| |
|