Anyone of there got a good Cone9-10 slip that can be poured on really
thick. I also like dunking pots in thick slip for finger wiping. I've got
some medicore ones but not one that blows my mind. I haven't got much of a
mind so your slip might be the one to blow it away. A slip with either
Helmar or Grolleg could be the cat's meow. I've got some of both and like
them in salt/wood.
Thanks for the trouble.