search  current discussion  categories  materials - misc 

tri calcium phosphate -corrections!

updated sun 31 aug 97

 

June Perry on mon 18 aug 97

Thanks Tom:

These old eyes read the wrong ingredient! Here's what I have to Tri-Calcium
Phosphate which on the lists I have has bone ash in parenthesis after it:

Ca3 : (PO4)2 Mol wt. 310, Equivalent wt. 103

I checked a few sources and they all give the same formula for Tri-Calcium
phosphate as bone ash. Some sources were Rhodes and Walker Ceramics.

Warm regards,