search  current discussion  categories  glazes - specific colors 

trying to get the blues

updated thu 31 oct 96

 

Alan Wainright on fri 18 oct 96

Hello, all!

I seem to recall in cruising through here about a week ago that I
saw some articles or discussion on a Blue Crackle raku glaze.
Does my memory serve correctly? If so, would anyone care to pass
this recipe on to me? We're having a raku firing at my wife's
ceramic shop to celebrate Halloween this year, & I'd like to take
my first experimental steps into glaze mixing... Thanks!

Looking forward to hearing from you...

Alan

WHampton@aol.com on sat 19 oct 96

I have this glaze from Clayart that might help.
CRACKLE RAKU (Light blue or copper)

Pemco Frit 25 80
Custer Feldspar 20
Copper Carb. 1

Good Luck
Wendy from Bainbridge Island WA