Someone posted a while back that they were looking for a clear glaze that
did not "milk" in thicker applications. This is a glaze that an Atlanta
potter gave to me to try out ! it is really good and consistent and
behaves nicely (compared to other clear glazes I have experimented.)

Richter Matte Clear ^6

Gerstley Borate 47.0
EPK (Kaolin) 20.0
Silica 27.0
Alumina Hydrate 6.0
----------
100.00

Hope this helps!

Amy Gossett in "Peachy" Rome, Ga. where the "hobbiers"
are all out to get me....NOT!
++++++++++++++++++++++++++++++++++++++++++++++++
"Reality is merely a crutch for those with a broken imagination..."
++++++++++++++++++++++++++++++++++++++++++++++++