gimme a laguna body

updated sat 7 apr 07

 

Megamelon on thu 5 apr 07


I want to switch to Laguna or Standard clay because of supplier =
proximity (Portland pottery location in MA). I'm still working out =
bodies and glazes, so it's a good time to experiment.

I'm mostly throwing, single firing,cone 10 in a wood fired kiln (will =
build when this latest snow and the ground thaws). Sheesh- can I put in =
any more unknowns here? Oh- working out glazes still, but want =
something that will show some good flashing. =20

How about BMix with grog (I ask because it's not standard for them to =
carry)?

Thanks
Paul Haigh