> http://picasaweb.google.com/SunnyDazeDesign/CoyoteGlazeTests?authkey=2X2ifbCN-N8
>
> Two glaze firings ago I over fired by 80-100F. Yikes. All of my glazes
> that I made looked like absolute crap. They were all matt glazes too so
> even worse results. The coyote glazes were not affected by being over-fired
> one bit. Not even in the slightest. And when I compared them to pieces
> fired to exactly cone 6, the results were identical!
>
> Truly amazed!
>
> --
> Lisa Elbertsen