Ivor and Olive Lewis on fri 20 apr 07
People who are interested in reduction firing and use an Oxyprobe might =
also be interested in the Ellingham Diagram.
The following site gives access to an tool that helps with thermodynamic =
calculations and an assessment of Oxygen partial pressures at elevated =
temperatures.
http://www.engr.sjsu.edu/ellingham/
There is also a diagram in Introduction to ceramics by Kingery et al.
Have a good weekend,
Ivor Lewis.
Redhill,
South Australia.
| |
|