Ivor and Olive Lewis on sat 21 apr 07


Dear John Connolly,

My suggestion would be to use commercial undergalze stains with the =
makers recommended flux. To get an even coating airbrush the material =
onto your greenware and cover with a hard transparent glaze after =
bisquing.

Using a copper cobalt glaze with strong reduction will give excellent =
purple hues but you may loose transparency.

Best regards,

Ivor Lewis.
Redhill,
South Australia.


.