Billie Mitchell on sun 22 apr 07
i have a freind who has lost his recipe for white crackle raku glaze. he has alot of frit 5301 and wants to use the same type of recipe that contains that frit.. if you have one please email me at livingspiritpottery@comcast.net.
thanks
billie mitchell
in georgia where spring has finally sprung.
--
livingspiritpottery@comcast.net
PO.BOX 2783
Acworth ga. 30102
Alisa Clausen on sun 22 apr 07
>i have a freind who has lost his recipe for white crackle raku glaze. he
has alot of frit 5301 and wants to use the same type of recipe that
contains that frit..
Hi Billie
What is in that Frit? Does it melt at around 700-800c? I was under the
impression that any frit around that melting point, plus maybe 20% Neph.
Sye or 10 %Borax and 10% Kaolin, plus and addition of 10% Ziropax, will
give a white crackle raku glaze. Even 100 Frit plus 10% Ziropax.
Do not know too much about Raku glazes, but have tried 100% Boron Frits
and then blended with 10% Kaolin, 10%Borax and the Zircopax and had a good
raku white crackle.
Best regards from Alisa in Denmark
| |
|