search  current discussion  categories  glazes - cone 8-10 

venturing into cone 10 gas

updated mon 30 apr 07

 

Randy McCall on sun 29 apr 07


I am going to venture into Cone 10 with my gas kiln and am looking for a
very forgiving Cone 8 to 10 Tenmoko Glaze that breaks iron and an oatmeal
glaze that will go with it.
Have been firing in electric. Using Phoenix clay from Highwater.


Appreciate any help getting started.


Randy
South Carolina