search  current discussion  categories  glazes - faults 

tried and true glaze begins shivering

updated wed 2 may 07

 

Snail Scott on tue 1 may 07


Oops! Ron Roy pointed out my recent brain fart!
To cure shivering, you need to REDUCE silica,
not add more (as I said yesterday). D'oh!