Alisa Clausen on wed 2 may 07
Amount Ingredient
15 Barium Carbonate
10 Gerstley Borate--1999
15 Wollastonite
39 Nepheline Syenite
10 Kaolin--EPK
11 Silica
100 Total
Unity Oxide
.209 Na2O
.061 K2O
.021 MgO
.472 CaO
.237 BaO
1.000 Total
.423 Al2O3
.115 B2O3
.003 Fe2O3
2.553 SiO2
.001 TiO2
0 P2O5
6 Ratio
8.3 Exp
| |
|