In a message dated 5/5/2007 7:53:56 P.M. Eastern Daylight Time,
Mudpitnyc@AOL.COM writes:

Kathleen,
I don't have a bead glaze but I do have two other low fire textural glaze
recipes.
Foam
Fritt 3110 63
wollastonite 9
bone ash 18
frit 3134 5
EPK 5
This glaze must be mixed thick and applied thick you could also add stains
and oxides for colors

Crawl
Barium carb 9
gertsley borate 19
magnesium carb 19
neph sye 28
EPK 16
flint 9

Cindy Gatto & Mark Petrin
The Mudpit
228 Manhattan Ave
Brooklyn, NY 11206
718-218-9424
_www.mudpitnyc.com_ (http://www.mudpitnyc.com/)







************************************** See what's free at http://www.aol.com.

Cindy Gatto on sun 6 may 07


Oh ummmm low fire range? just joking! ^06-04 for the crawl ^04 for the foam
by the wat the foam glaze can get very foamy

Cindy Gatto & Mark Petrin
The Mudpit
228 Manhattan Ave
Brooklyn, NY 11206
718-218-9424
_www.mudpitnyc.com_ (http://www.mudpitnyc.com/)
mudpitnyc@aol.com



************************************** See what's free at http://www.aol.com.