search  current discussion  categories  techniques - casting 

glazing steel, cast iron

updated sun 20 may 07

 

Terrance Lazaroff on fri 18 may 07


hi all;

Anyone in the group glaze steel or cast iron successfully?

Terrance

Ivor and Olive Lewis on sat 19 may 07


Dear Terrance Lazaroff ,

Steel and Cast Iron are regularly give ceramic surfaces. The process is =
called "Vitreous Enamelling". The materials can be obtained from W. G. =
Ball in Staffordshire, England.

Best regards,

Ivor Lewis.
Redhill,