Richard Urban on mon 4 jun 07
hi. I'm looking for a basic white cone 5 slipglaze. I've tested a few recipes but they have been coming out too rough. I was hoping to to flux it a bit so it will have just a bit of sheen to it. Haven't had much luck.
Thanks for your help
Richard
---------------------------------
Ready for the edge of your seat? Check out tonight's top picks on Yahoo! TV.
MacIntire, Matt on tue 5 jun 07
Richard, have you worked any with Ravenscrag slip? By itself it melts
at cone 10 and is pretty white. They have very simple recipes for cone
6 that are fluxed with about 20% of a boron frit.
http://ravenscrag.com
Lots of cone 6 recipes with photos, application recommendations and