I know normally we don't want glazes to crawl let alone bead, but
to get an intense colour from an overglaze this seems to work -
cf. the glaze system I'm trying to duplicate at
http://sankey.ws/pottery2.html

So, how might it be done?

By the way, I'm not limited to cone 04 for the overglaze, it just
has to be a truly melted glaze to be functional and foodsafe, and
to fire at enough less than cone 6 that the main glaze doesn't
melt.