rant: examine your bottom! not just bottoms, think raku.

updated thu 21 jun 07

 

Terrance Lazaroff on tue 19 jun 07


I just have to add to this Rant. Many potters do raku and they do not
seal their work nor do they tell the client that it will weep if filled
with water. A very nice grand piano destroyed because of water. Another
well to do customer gone.

Terrance