glaze problem with amaco galze-text.amber??

updated sat 30 jun 07

 

Annette Libby on fri 29 jun 07


Hi everyone! Just done a load of Cone 5,some of the pieces were glazed with
a Amaco Sahara liquid Glaze called Textured Amber. I used this glaze before
and had no problems,this was a newly opened container and for some reason it
came out very funky looking and not at all like I had expected.All the
pieces glazed with this Glaze came out completely dull looking,non transparent,not
shiny at all.What did I do wrong? The other Glazes that I used on the same
piece came out fine. Thanks in advance! Annette Libby.