search  current discussion  categories  glazes - specific colors 

more waterfall brown test results

updated sat 30 jun 07

 

Jamie Yocono on fri 29 jun 07


Hi everyone,

I'm so glad I'm getting the daily digest again. I felt a little isolated
without it.

As some of you know, I've been trying to develop a Waterfall Green, based on
the WF Brown recipe in Ron and John's book. I've been corresponding with a
few people off-line regarding some of the tests I've been running. A few
people suggested I share those results, so I posted some pictures on my blog:
http://wooditis.blogspot.com/

I think I'm getting pretty close to the green I want, it's quite exciting.

That's the good news.

The bad news is- once again, I'm having kiln problems. I'm getting an error
message regarding my thermocouple. :( As Roseanne Roseannadanna used to
say- it's always something.

Jamie in Vegas