John Sankey on fri 6 jul 07
The following glaze is attributed to Richard Zakin at
http://lsv.ceramics.org/scripts/wa.exe?A2=ind9907&L=CLAYART&P=R52791
Emerald Transparent
nepheline syenite 51g
Gerstley borate 22g
Wollastonite 14g
EPK 8g
zinc oxide 3g
copper carbonate 3g
titanium dioxide 2g
As published, this is a watery glaze that runs almost completely
off the pot at cone 6. Does anyone have the Zakin book in which
it was published? Was it really for cone 6?
--
(Add 'Byrd' to the subject line of your reply to get through my spam filter)
| |
|