Laura: I am a member of a pottery co-op with a cement floor in one of its
work areas. Every other year we thoroughly clean the floor and apply a good
quality cement sealer (purchased from a local paint dealer) to stop the
cement dust from circulating. This floor is washed about twice a month and
stands up extremely well under heavy usage.