Ron Roy on tue 21 aug 07
Thanks for catching that John - exactly right.
RR
>"The alumina in this glaze [Reitz Green] is way up there at .86 -
>the upper limits for a cone 10 glaze are commonly 5.5 so I am
>thinking this is going to be very hard to melt."
>
>I assume Ron meant .55, not 5.5
>
>Its expansion is also very high at 7.0; most stonewares are lower
>than this - mine for example is 6.6, so I would think crazing is
>probable except on high-expansion porcelains or if applied very thin.
>
>--
>(Add 'Byrd' to the subject line of your reply to get through my spam filter)
>
>______________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
Ron Roy
RR#4
15084 Little Lake Road
Brighton, Ontario
Canada
K0K 1H0
| |
|