Hmmmmm..... I wonder if that would work with my reclaim???
That 5 gal. bucket frequently goes various degrees of black!

Gayle Bair
Bainbridge Island, WA
Tucson, AZ
http://claybair.com

-----Original Message-----
From: Angela Davis

Myrna,
At NCECA this year I picked up the tip of using
copper carb as a sanitizer in your paperclay slop.
I add a heaping teaspoon to a 5 gal bucket of the
paper slip. This amount works for me and is not
enough to color the clay.
The advantage over bleach is that it does not degrade
out of the mix.

Angela Davis