Ron Roy on tue 21 aug 07


Jamie would like to hear from anyone who has be able to make a green
version of waterfall.

jamie@wooditis.com

She also makes some pretty special furniture which you can see on her
website - which I also found special.

www.wooditis.com

RR

Ron Roy
RR#4
15084 Little Lake Road
Brighton, Ontario
Canada
K0K 1H0

Charlotte on wed 22 aug 07


The waterfall green glaze I made was a pretty color but had pin
holes. The pin holes dissapeared when I tested it over another base
glaze.

Charlotte Wiley

--- In clayart@yahoogroups.com, Ron Roy wrote:
>
> Jamie would like to hear from anyone who has be able to make a
green
> version of waterfall.
>
> jamie@...
>
> She also makes some pretty special furniture which you can see on
her
> website - which I also found special.
>
> www.wooditis.com
>
> RR
>
> Ron Roy
> RR#4
> 15084 Little Lake Road
> Brighton, Ontario
> Canada
> K0K 1H0
>
>
_____________________________________________________________________
_________
> Send postings to clayart@...
>
> You may look at the archives for the list or change your
subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@...
>