Greg McRitchie on sun 26 aug 07
I would appreciate some input on some raw Ochre that I found on Vancouver Island this summer. I have posted the details and some good pics on my brand new blog. (Don't laugh, I'm new at this blog stuff). It's called "Another Blog On The Fire" http://fireandmud.blogspot.com/ Anyway; I have quite a bit of material sampled and I would like some suggestions on how to go about processing and testing it. I have a large gas kiln and I fire to cone 10-11 reduction. Any help or suggestions on the tests or the blog would be welcomed. I plan on doing quite a bit of posting on the blog about how I do the things I do with an emphasis on throwing. I have been a full time potter since 1982 It also looks like there is a deposit of Copper in the same location that I did not notice until I saw the pictures because I forgot to bring a flashlight. Duhhh!
Look at the pic on the blog and let me know what you think.
Thanks:
Greg McRitchie
Mudslide Stoneware
Alberta Canada
http://fireandmud.blogspot.com/
---------------------------------
Sick sense of humor? Visit Yahoo! TV's Comedy with an Edge to see what's on, when.
Angela Davis on mon 27 aug 07
Greg,
If you could create a glaze as beautiful as that cave wall
you would indeed have something.
Thanks for sharing.
Angela Davis
In Homosassa
----- Original Message -----
From: "Greg McRitchie"
To:
Sent: Sunday, August 26, 2007 7:32 PM
Subject: Ochre and Copper deposit
>I would appreciate some input on some raw Ochre that I found on Vancouver
>Island this summer. I have posted the details and some good pics on my
>brand new blog. (Don't laugh, I'm new at this blog stuff). It's called
>"Another Blog On The Fire" http://fireandmud.blogspot.com/ Anyway; I
>have quite a bit of material sampled and I would like some suggestions on
>how to go about processing and testing it. I have a large gas kiln and I
>fire to cone 10-11 reduction. Any help or suggestions on the tests or the
>blog would be welcomed. I plan on doing quite a bit of posting on the blog
>about how I do the things I do with an emphasis on throwing. I have been a
>full time potter since 1982 It also looks like there is a deposit of
>Copper in the same location that I did not notice until I saw the pictures
>because I forgot to bring a flashlight. Duhhh!
>
> Look at the pic on the blog and let me know what you think.
>
> Thanks:
> Greg McRitchie
> Mudslide Stoneware
> Alberta Canada
> http://fireandmud.blogspot.com/
>
>
>
> ---------------------------------
> Sick sense of humor? Visit Yahoo! TV's Comedy with an Edge to see what's
> on, when.
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>
>
> --
> No virus found in this incoming message.
> Checked by AVG Free Edition.
> Version: 7.5.484 / Virus Database: 269.12.8/973 - Release Date: 8/25/2007
> 5:00 PM
>
>
Greg McRitchie on mon 27 aug 07
Thank you for the kind comments and suggestions. I have added some more pics of the deposit on my blog http://fireandmud.blogspot.com/ . I am interested in any ideas about testing the copper. If any one has had experience with raw copper I would love to hear about it. Somehow the little baggies of green powder I get from Ceramics Canada don't seem quite as sexy as digging the stuff out of the side of a hill but the processing may be impractical for a relatively small scale potter without some industrial equipment. I don't know, that's why I'm asking.
Thanks
Greg McRitchie
Mudslide Stoneware
Alberta Canada
http://fireandmud.blogspot.com/
---------------------------------
Choose the right car based on your needs. Check out Yahoo! Autos new Car Finder tool.
Greg McRitchie on tue 28 aug 07
Thank you for the kind comments and suggestions. I am interested in any ideas about testing the copper. If any one has had experience with raw copper I would love to hear about it. Somehow the little baggies of green powder I get from Ceramics Canada don't seem quite as sexy as digging the stuff out of the side of a hill but the processing may be impractical for a relatively small scale potter without some industrial equipment. I don't know, that's why I'm asking. I have added some more pics of the deposit on my blog http://fireandmud.blogspot.com/ .
Thanks
Greg McRitchie
Mudslide Stoneware
Alberta Canada
http://fireandmud.blogspot.com/
---------------------------------
Ready for the edge of your seat? Check out tonight's top picks on Yahoo! TV.
| |
|