Hello,
I am looking to coat the K26 on the chamber of my wood fired kiln that I =
am building. John Chalke used a mix of alumina, zircopax and frit on his =
soda wood kiln and says that it worked great , but does not remember the =
proportions he used. I am planning to test various mixes in our gas kiln =
but that will just tell me how it melts and not how it will stand up =
long term. Anyone have a any experience with this mix or any other for =
IFB?
Regards,
Eva Gallagher
Deep River, Ontario