search  current discussion  categories  glazes - cone 04-06 

boron blue clouding at ^04

updated mon 3 sep 07

 

Julie Michaud on sun 2 sep 07


I'm having a little trouble with my ^04 clear honey glaze. It's going
cloudy-blue anywhere the application is a little thick. I'd really like to
adjust this to be a more forgiving clear glaze, but really don't know where
to start. I can't seem to find any information on this topic on the web.

Here's my recipe:

Gerstley Borate 30
Frit 3124