Angela Davis on wed 12 sep 07


I am down to the bottom of my ITC container. =20
I have a fair amount of granules left. I've been adding water and =
stirring it back up
but wonder if there is a limit as to how many times you can do this.

I figure I am using up all the fine particles that make the coating =
stick.

If so would adding some EPK or other ingredient make the grains stick
again? Or should I just buy fresh?

Angela Davis

In Homosassa