Paul Borian on mon 10 sep 07


I need to have a chemical analysis done on the local clay I use for my
slip glazes so I can start using glaze calculation software to help make
different variations of the glaze. Can anyone recommend a lab that would
do this and tell me what the cost is?

Thanks,

Paul

Paul Herman on tue 11 sep 07


Paul,

Try ALS Chemex. Last time it was $120 for four analyses. They were
prompt and very professional.

http://www.alschemex.com/

Best,

Paul Herman

Great Basin Pottery
Doyle, California US
http://greatbasinpottery.com


On Sep 10, 2007, at 7:03 PM, Paul Borian wrote:

> I need to have a chemical analysis done on the local clay I use for my
> slip glazes so I can start using glaze calculation software to help
> make
> different variations of the glaze. Can anyone recommend a lab that
> would
> do this and tell me what the cost is?
>
> Thanks,
>
> Paul
>