search  current discussion  categories  materials - rutile 

bob anderson's rutile blue

updated mon 24 sep 07

 

Robert W. Anderson on sun 23 sep 07


Bob Anderson's rutile blue plates.
(Click link below).
Mel's orange over Rhodes 32.
Fired to cone 10 or 11 with mild
reduction. The blue seems to be
more pronounced at cone 11 and
varies with thickness. Soaking at
1950 deg. for half to one hour
flattens the glaze and eliminates
pinholes.
Trying to help ya out Mel...I know you
were busy at the farm this weekend.

Bob
-------------
http://webpages.charter.net/rwapottery/index.html