Eleanora Eden on mon 24 sep 07


I use my slip clay as a slip, both with ^06 slip on lowfire work and ^1 slip
for ^1 work. I have many times painted a coat of slip onto bisque and
then bisqued again before any further work. Has always done fine for me.

Eleanora

>I've been taught that once bisqued, you can forget about the slip. It
>won't stick. I know that once bisqued you can forget about terra sig -
>it absolutely will not stick and then sloughs off in nasty patterns.

--