search  current discussion  categories  people 

attn: ron roy - black glaze #2 var. 1 (diane woloshyn)

updated fri 19 oct 07

 

John Rodgers on thu 18 oct 07


Dear RR:

I have seen this glaze recipe somewhere, but for the life of me I cannot
find it. I have been through the archives,and on the MC website, but
didn't see it. When I did see the discussion, Diane Woloshyn's name was
in the discussion.

Would you mind sending me a link or something for that glaze. Sure would
appreciate it.

Thanks,

John Rodgers
Chelsea, AL

Lee Love on thu 18 oct 07


I apologise for not be RR, but this was on the web here:

http://www.frogpondpottery.com/glazestability/glaze0007.html

Frit 3132 26.0
Kona f-4 21.0
Whiting 6.0
Talc 3.0
EPK 17.0
Silica 27.0

Bent. 2.0
R.I.Ox 9.0
Cobalt carb 1.0
Mason 6600 1.0


--
Lee in Minneapolis, Minnesota USA

http://mashikopots.blogspot.com/

"For a democracy of excellence, the goal is not to reduce things to a
common denominator but to raise things to a shared worth."
--Paolo Soleri

John Rodgers on thu 18 oct 07


Lee,

Thanks. Don't know how I missed it, but that's the one.

Regards,

John

Lee Love wrote:
> I apologise for not be RR, but this was on the web here:
>
> http://www.frogpondpottery.com/glazestability/glaze0007.html
>
> Frit 3132 26.0
> Kona f-4 21.0
> Whiting 6.0
> Talc 3.0
> EPK 17.0
> Silica 27.0
>
> Bent. 2.0
> R.I.Ox 9.0
> Cobalt carb 1.0
> Mason 6600 1.0
>
>
>