mel jacobson on fri 26 oct 07


axner, i am sure will always carry itc.
he has been a huge supporter of the product, and
is the major distribution point now for potters.

feriz is still doing a great deal of industrial/military work both
in kiln design and itc application. he does not want to
sell itc a quart at a time out of his factory. axner does that.

feriz has been designing/building large kilns in mexico, south korea
and has some work i believe in china. large meaning...over 10,000
square feet. modules with itc coating. he also is doing some very
interesting kilns for the navy...heat treating for special metals.
very high temp. nasa is now using itc on their launch pads.
so.
i know he is still very active.
mel