question about sapphire blue glaze.....figured out what the problem

updated sat 27 oct 07

 

Nancy on fri 26 oct 07

was!

I can't find the thread but several people offered some advice for the
Ron Roy's sapphire glaze that just didn't seem to work for me so I tried
to thicken it. This glaze seems to do so much better when it is
applied thickly and if not over fired it doesn't run too much.

Using my baster, I sucked all the water off the top of the glaze bucket
and then mixed it up, glazed the pieces and OMG! back to the beautiful
glaze!!!!

Woohoo...thanks to everyone for the advice