search  current discussion  categories  materials - misc 

high potash feldspar

updated mon 5 nov 07

 

John Sankey on sat 3 nov 07


Feldspars can contain up to 17% potash by weight, but the only
potash feldspars I can find locally or at major mail order places
are Custer's and G-200, both of which are less than 11% potash.
Does anyone know of a mail source of high-potash feldspar?

--
Include 'Byrd' in the subject line of your reply
to get through my spam filter.

John Britt on sun 4 nov 07


John,

I would contact the Custer mine in Custer South Dakota and ask about dental
feldspar.

Hope it helps,

John Britt
www.johnbrittpottery.com