Some months ago I asked for a box of cone 10 Laguna
B mix from my supplier. Now I have changed my mind and
have decided to stick with my usual B mix cone 5-6.=20
I am passing the high fire to a friend and want to be sure
it is high fire, cone 10.
It is unclear on the unopened box. It says, in stamped letters, WC379
B mix cone
further over, above the Laguna logo, are the also stamped numbers 31270.
My boxes of cone 5 say cone 5, but not on the other box.
I am 90% sure it is cone 10, but want to be 100%.
Could someone from Laguna tell by the code number if it is indeed?
Thanks,
Lela
=20
_________________________________________________________________
Have fun while connecting on Messenger! Click here to learn more.
http://entertainment.sympatico.msn.ca/WindowsLiveMessenger=

Nancy on sun 25 nov 07


Lela

Yes it is cone 10. WC379 is BMix cone 10

you can see this at the link below:

http://www.lagunaclay.com/clays/northeastern/cone10.php

Nancy

lela martens wrote:
> Hi,
>
> Some months ago I asked for a box of cone 10 Laguna
> B mix from my supplier. Now I have changed my mind and
> have decided to stick with my usual B mix cone 5-6.
> I am passing the high fire to a friend and want to be sure
> it is high fire, cone 10.
> It is unclear on the unopened box. It says, in stamped letters, WC379
> B mix cone
> further over, above the Laguna logo, are the also stamped numbers 31270.
> My boxes of cone 5 say cone 5, but not on the other box.
> I am 90% sure it is cone 10, but want to be 100%.
> Could someone from Laguna tell by the code number if it is indeed?
> Thanks,
> Lela
>
> _________________________________________________________________
> Have fun while connecting on Messenger! Click here to learn more.
> http://entertainment.sympatico.msn.ca/WindowsLiveMessenger
> ______________________________________________________________________________
> Clayart members may send postings to: clayart@lsv.ceramics.org
>
> You may look at the archives for the list, post messages, or change your
> subscription settings here: http://www.acers.org/cic/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots2@visi.com
>
>

James and Sherron Bowen on sun 25 nov 07


Try this
http://www.lagunaclay.com/catalog/


----- Original Message -----
From: "lela martens"
To:
Sent: Saturday, November 24, 2007 10:30 PM
Subject: someone from Laguna co.?


Hi,

Jon Pacini on tue 27 nov 07


Greetings All ---Hi Lela--- the clay you have is WC 379 B-mix ^10, as stated
earlier, you can find it on the Laguna Web site---just wanted to make it
"official"
Best regards,
Jon Pacini
Clay Manager
Laguna Clay Co

lela martens on tue 27 nov 07


Many thanks to J&S Bowen,and Nancy, for the=20
help and taking the time.
Lela, where it`s COLD outside and getting colder.
=20
_________________________________________________________________
Are you ready for Windows Live Messenger Beta 8.5 ? Get the latest for free=
today!
http://entertainment.sympatico.msn.ca/WindowsLiveMessenger=